Figure 3From: The effect of a new formaldehyde-free binder on the dissolution rate of glass wool fibre in physiological saline solution Average continuous draw glass fibre diameter decrease with time. The average fibre diameter decrease with dissolution time from measurements on eight individual fibres for continuous draw glass fibre samples 1 and 2. The indicated error is typical of a set of measurements on 8 individual fibers.Back to article page