Skip to main content

Table 2 H2O2 decomposition rate constants (ktot) and corresponding half-life times determined by fitting the H2O2 concentration data presented in Fig. 4 to the first order rate equation: \( {Rate}_{\left({H}_2{O}_2\right)}=-\frac{d\left[{H}_2{O}_2\right]}{dt}={k}_{tot}\left[{H}_2{O}_2\right] \)

From: Identifying the reactive sites of hydrogen peroxide decomposition and hydroxyl radical formation on chrysotile asbestos surfaces

Experiment Nr.

Treatment

First order rate constant ktot [h− 1]

R2

t1/2 [h]

1

MOPS pristine fibers

6.2*10−3

0.998

112

2

MOPS blank-altered fibers

4.2*10−3

0.996

165

3

MOPS DFOB-altered fibers

2.5*10−3

0.956

277

4

MOPS DFOB-altered fibers + 0 μmol g− 1 Fe

2.5*10− 3

0.944

277

5

MOPS DFOB-altered fibers + 3 μmol g− 1 Fe

2.7*10− 3

0.992

257

6

MOPS DFOB-altered fibers + 30 μmol g− 1 Fe

3.5*10− 3

0.982

198

7

MOPS DFOB-altered fibers + 300 μmol g− 1 Fe

5.3*10− 3

0.986

131

8

MOPS buffer (no fibers) panel a & c of Fig. 4

1.2*10− 3

0.931

578

9

MOPS blank-altered fibers + 0 μmol g− 1 Fe

4.2*10− 3

0.979

165

10

MOPS blank-altered fibers + 3 μmol g− 1 Fe

4.2*10− 3

0.983

165

11

MOPS blank-altered fibers + 30 μmol g− 1 Fe

4.9*10− 3

0.988

142

12

MOPS blank-altered fibers + 300 μmol g− 1 Fe

6.0*10− 3

0.995

116

13

MOPS buffer (no fibers) panel d of Fig. 4

1.4*10− 3

0.995

495

14

NaOH pristine fibers

46.7*10− 3

0.936

14.8

15

NaOH blank-altered fibers

41.5*10−3

0.995

16.7

16

NaOH (no fibers)

1.0*10−3

0.772

693